新闻中心
PP (polypropylene) plastic has extremely low surface energy and is difficult to wet. Ordinary EVA hot melt adhesive particles stick directly, which is basically a “false adhesion” and can be easily peeled off. This is the most common pitfall: thinking that hot melt adhesive is omnipotent, but the PP adhesive falls off completely.

| Scene | method |
|---|---|
| PP packaging adhesive | Select PO type/modified special particles+surface treatment |
| PP and paper composite | Specialized formula for soaking paper while grabbing PP |
| Small fixed area | Apply adhesive after primer for greater stability |
Q: Does Sunlife have particles that can stick to PP?
Answer: Yes, Guangzhou Sunlife Trading recommends specialized models based on PP type and sends samples.
Q: Can the surface stick without treatment?
Answer: Difficult, it is recommended to at least do corona discharge, which has low cost and good effect.
Q: Is PE as difficult to stick as PP?
Answer: Similar, both belong to polyolefins and require specialized formulas.
PP adhesive overturned, sent the material sample to Guangzhou Sunlife Trading, and Sunlife hot melt adhesive provided the formula+process combination.
The feasibility of reheating and reworking hot melt adhesive after solidification depends on the degree of degradation of the adhesive performance after the secondary heating. This article explains the typical changes of EVA hot melt adhesive after multiple heating, the key points of rework operation, and why PUR cannot be reworked.
Mechanical anchoring theory:Adhesive must penetrate into the gaps on the surface of the adhered object and eliminate the air adsorbed on its interface in order to produce adhesive effect.. The mechanical theory is very convincing in explaining the bonding of porous materials such as wood and materials with rough surfaces, and has been verified in […]
What are the applications, uses, and advantages of hot melt adhesive? Hot melt adhesive is widely used in various industries. Here are some of the main industries that benefit from hot melt additives. Electronics:Electronic innovation affects almost every field of our lives.. The formula currently under development helps promote electrical interconnection, provide critical protection, and […]
What should I do if the hot melt adhesive particles are not firmly attached to the coated paper? Direct answer: The root cause of the poor adhesion of laminated paper is mostly due toLow membrane surface energy, glue not eating paper fibers, poor coordination between opening time and compressionThese three points. The surface of laminated […]