When purchasing hot melt adhesive, RoHS reports are often used as a “compliance pass”. But the short lines of ‘ND’ in the report actually prove and cannot prove something, and many people are actually confused. This article uses Sunlife’s 2026 SGS RoHS report to explain each item clearly.
First, let’s talk about the most easily misunderstood point. This report is aimed at a submission for inspectionHot melt adhesive sample (sample description: white material)The original report clearly states:
The results of this report are only responsible for the samples tested
So,cannotUnderstand it as’ All Sunlife hot melt adhesive models have passed RoHS’. The correct statement is:This report certifies the compliance of the submitted samples in the listed ten items. When making purchases, you should request corresponding accompanying reports based on the model and batch you have purchased.
| item | content |
|---|---|
| testing agency | SGS Standard Technical Services Co., Ltd. Guangzhou Branch |
| Report Number | CANEC26008641201 |
| Reporting Date | April 15th, 2026 |
| SGS job number | GZP26-010021 |
| Sample collection/testing cycle | Sample collection on April 10, 2026; 2026-04-10~04-15 testing |
| Sample Name | hot melt adhesive |
| Sample description | White material (SGS sample ID: CAN26-0086412-0001. C001) |
| Client | Foshan Jucai New Materials Co., Ltd. (Sunlife Hot Melt Adhesive Production Base/Historical Associated Entity) |
This report is based onEU RoHS Directive 2011/65/EU and its amended Directive (EU) 2015/863Covering ten substances:
In terms of limit values,Cadmium is 100 mg/kg, while the other nine are all 1000 mg/kg。
The detection method refers to the IEC 62321 series (ICP-OES/AAS, UV Vis, GC-MS). The results are as follows:
| Testing Items | limit | unit | MDL (detection limit) | result |
|---|---|---|---|---|
| Lead Pb | 1000 | mg/kg | 2 | ND |
| Mercury Hg | 1000 | mg/kg | 2 | ND |
| Cadmium Cd | 100 | mg/kg | 2 | ND |
| Hexavalent chromium Cr (VI) | 1000 | mg/kg | 8 | ND |
| Sum of polybrominated biphenyls PBB | 1000 | mg/kg | — | ND |
| Sum of polybrominated diphenyl ethers PBDE | 1000 | mg/kg | — | ND |
| DEHP | 1000 | mg/kg | 50 | ND |
| BBP | 1000 | mg/kg | 50 | ND |
| DBP | 1000 | mg/kg | 50 | ND |
| DIBP | 1000 | mg/kg | 50 | ND |
All ten items are ND (not detected).
ND = Not Detected, pointBelow the Method Detection Limit (MDL)It is not ‘content exactly 0′. In other words, it is’ undetectable under existing detection capabilities’ rather than ‘absolutely non-existent’.
The practical significance for the purchaser is:This sample for inspection meets the limit requirements of RoHS ten itemsIt can serve as evidence of supplier compliance capability. but itCannot replaceThe report of the model and batch of goods you want to buy.
Q: Does RoHS display ‘not detected’ mean these substances are completely absent?
A: Not equal to absolute zero. ND refers to being below the detection limit of the instrument, which means that it has not been detected within the detection capability range.
Q: Can a RoHS report represent all hot melt adhesive models?
A: I can’t. This report is only responsible for the sample submitted for inspection, and corresponding reports for other models/batches need to be provided separately.
Q: How to obtain compliance documents from suppliers during procurement?
A: Tell the other person about youModel+BatchRequest the accompanying RoHS report corresponding to this batch; If used in formal settings, indicate the purpose of the required report.
Q: Does Sunlife have RoHS documentation?
A: Yes, there is. The 2026 SGS RoHS report (number CANEC26008641201) shows that none of the ten items in the hot melt adhesive samples were detected, and can be provided upon request.

Guangzhou Sunlife Trading Co., Ltd. specializes in the supply and application services of hot melt adhesive, which is manufactured by Foshan Jucai Base (a historical affiliated entity). Compliance and testing data shall be provided based on the actual model/batch and shall not be expressed beyond the scope.
First of all, let’s talk about the results: a tourism printing factory in East China produces foldable map brochures, with 55 gram ultra-thin floor drawings on the inner pages. Originally, using ordinary rubber particles often resulted in glue penetration and cracking at the folds. After switching to Sunlife hot melt adhesive thin paper special low-temperature […]
How to prevent clothing tags from falling off with hot melt adhesive particles? A Guangzhou clothing factory was repeatedly returned by e-commerce customers due to the detachment of tags. The hanging tag is easy to loosen when tied with wire and easy to curl when used with adhesive tape. Later on, hot melt adhesive particles […]
When it comes to hot melt adhesive, many people only know how to stick it by hand or cardboard boxes, but they don’t know that it has already penetrated hundreds of industries such as printing, binding, packaging, home furnishings, light industry manufacturing, electronic auto parts, etc. It is a “universal adhesive” for industrial production and […]
Are friends who work in printing, binding, and brochure production always troubled by these problems: opening the glue when flipping pages on copperplate paper books, yellowing of the glue layer and low texture, and equipment for drawing and sticking glue during high-speed production? In fact, 90% of the problems lie in the selection of hot […]