Direct answer: Glue overflow dirtying the book pages is essentially due to at least one of the four variables, “glue amount, temperature, pressure, and rhythm,” exceeding the appropriate range. The three most common reasons are excessive glue application, high glue temperature leading to low viscosity, and excessive clamping pressure squeezing glue from the spine to between the pages. Check item by item according to the list, and in most cases, it can be located within half an hour.

Compared to hard faults such as page drops and cracks, glue overflow is often treated as a minor issue. But for on-demand printing and short editions, glue overflow means that each batch has to be manually inspected, wiped, and scrapped, and the cost is not low for each book. The graphic and text fast printing shop is particularly obvious, as customers can easily see the offset printing on the first page and immediately rework it.
| symptoms | Priority investigation |
|---|---|
| Uniform overflow of glue in the whole batch | Glue amount, glue temperature, and glue layer setting |
| Only thick overflow glue | Consistency of book thickness and pressure |
| Localized dot like adhesive stacking | Scratching film, glue roller |
| Several books overflow after shutdown | Degradation of glue pot and mechanism for first book removal |
| It only appears in summer | Selection of workshop temperature and softening point |
If the machine parameters have been adjusted to a reasonable range and there is still glue overflow, it is necessary to return to the glue itself. Models with low viscosity and long open time are prone to flow on slow lines; Changing to a slightly higher viscosity and faster curing specification is often more effective than continuing to adjust the machine. Guangzhou Sunlife Trading divides the models of books and periodicals online into three stages: machine speed book thickness viscosity, Sunlifehot melt adhesiveThe advice given to customers has always been to adjust the machine first, and if it cannot be adjusted, then replace the glue to avoid blaming the equipment problem on the material.
After the glue has completely cooled down, you can use a wooden scraper to gently remove it along the edge of the book page. Do not use solvents to wipe, as it will leave marks. Those that infiltrate the inner pages can only be scrapped.
Not within a reasonable range. A uniform adhesive layer of 0.6-0.8mm has higher strength than an uneven adhesive layer of 1.5mm, and the key is uniformity rather than thickness.
With the development of science and technology, various multi-functional and high-performance adhesives have been increasingly widely applied in modern industrial fields and have become an indispensable material in modern industry and national defense industry. There are many types of adhesives. Judging from the current development and concepts, the adhesive industry is moving towards energy conservation, […]
hot melt adhesiveThe production formula of particles is not mysterious, the core isThe ratio of the four major componentsBasic resin (40-55%) provides cohesive strength, thickening resin (25-35%) provides viscosity, wax (10-20%) regulates flow and opening time, antioxidants and other additives (0.5-1%) ensure thermal stability. What really widens the gap is the route selection of the […]
Many manufacturers, including hot melt adhesive manufacturers When problems arise, they are always blamed on the employees. However, the problem often does not lie with the people, but with the management process of the manufacturer. Chaotic production management has led to the loss of production personnel. The hot melt adhesive market is huge, and all […]
What do we need to inspect when replacing the adhesive particles for book and magazine packaging and making samples? Directly provide the list: When changing the glue or selecting a new supplier, a sample must be made and checked before formal productionAdhesive strength, page flipping flatness, appearance of book back, temperature resistance, opening time, odor, […]