新闻中心
A clothing accessory factory produces brand tags and hanging cards, using Hot melt adhesive granules Stick the cardboard and rope buckle firmly. The complaints are concentrated on: about 6% of the hang tags have peeled off after transportation, and customers have failed to scan the code for price verification.

Guangzhou Sunlife trade technician suggests that the adhesive should be applied to the “two ear positions” of the rope buckle seat instead of the center, so that the tension can be dispersed along the ear positions; Replace with specialized granules with high initial adhesion and adhesive film surface; The coating amount is fixed at 0.25 g/point and controlled by a dispensing valve. Sunlife hot melt adhesive provides a comparison sample for bonding laminated cardboard, confirming that the damaged surface of the new material is on the paper fiber.
| indicator | Before renovation | after renovation |
|---|---|---|
| Glue opening rate | 6% | 0.4% |
| Poor appearance | Excessive overflow of glue | Basically none |
| customer complaint | Starting from monthly | Approaching zero |
Stick to the right position and select the right adhesive, which is more effective than simply adding the right amount of adhesive.
Q1: Do laminated tags require special adhesive?
Ordinary EVA difficult to film surface should choose adhesive film models.
Q2: Is it harder to apply more glue?
Excessive overflow of glue can lead to dirtiness and virtual adhesion, and the key lies in the location and quantity.
Customer background and challenges A textbook printing factory in Hunan has taken on an order for 200000 teaching aids with adhesive packaging, with a delivery time of only 15 days. The adhesive packaging line needs to work continuously in three shifts without stopping. Previously used a certain brandHot melt adhesive granulesAfter 8 hours of continuous […]
Are friends who work in printing, binding, and brochure production always troubled by these problems: opening the glue when flipping pages on copperplate paper books, yellowing of the glue layer and low texture, and equipment for drawing and sticking glue during high-speed production? In fact, 90% of the problems lie in the selection of hot […]
Hot melt adhesive granulesHow long should I preheat before starting up? The new operator Xiao Wang was in a hurry to rush the goods in the morning. As soon as the glue tank reached 160 ℃, he poured particles into it and opened the line. As a result, the first fifty books had blank glue […]
Case Background A factory that makes color boxes, in order to make the sealing glue line and the box of the same color, hides the seams and makes them transparentHot melt adhesive granulesAdd color masterbatch and adjust to deep red. After going online, the glue line became blurred, blocked the gun, and there were also […]