新闻中心
A small household appliance factory’s finished product boxes weigh 18 kilograms per box and are stacked in six layers in the warehouse. Use the original oneHot melt adhesive granulesAfter sealing and passing the factory inspection, the bottom box can be stored in the warehouse for two weeks. The seams of the top cover of the bottom box are gradually pushed open, forming a 2-3cm “mouth opening”. The cost of rework and resealing is not small. The problem lies in only assessing the sealing strength, without assessing the creep resistance under long-term stacking.

Technicians from Guangzhou Sunlife Trading brought samples to the factory for a control experiment: the original adhesive was changed to continuous adhesive strips along both sides of the box mouth, and the amount of adhesive applied was increased from 0.8g to 1.4g/box. At the same time, the heavy-duty sealing brand with high holding viscosity and softening point above 95 ℃ was replaced. Sunlife hot melt adhesive provides comparative data on the adhesion of three grades at a constant temperature of 40 ℃, and directly selects the one that meets the six layer stacking requirements.
| project | original plan | adjusted |
|---|---|---|
| Six layer stacking for 14 days | Bottom layer about 3.5% open mouth | 0 mouths open |
| Maintain a constant temperature of 40 ℃ for 7 days | Significant displacement of seams | No displacement |
| 1-meter drop | Qualified | Qualified |
| Cost of glue per box | benchmark | +0.6 points per box |
The conclusion is very solid: heavy box stacking does not focus on instantaneous tensile strength, but on the adhesion and creep resistance at high temperatures; Each box of glue costs less than a penny more, saving the entire batch of rework.
One is to inform the supplier of the actual working conditions: single box weight, stacking layers, maximum warehouse temperature, and storage period, which determine the direction of the brand; Secondly, it is required to conduct simulated stacking verification by placing heavy weights on the sample box for one to two weeks, which is closer to reality than the instantaneous tensile force in the laboratory; Thirdly, the width of the box opening overlap should also be taken into consideration. When the overlap is too narrow, even the best glue cannot withstand the stretching force.
Q1: What are the main indicators for selecting adhesive for heavy-duty boxes?
Check the adhesion and softening point, and request the supplier to provide retention data at high temperature and constant temperature, rather than just looking at tensile strength at room temperature.
Q2: Can stacking layers be solved by adding glue?
Adding quantity is helpful but limited. When the adhesive type is incorrect, priority should be given to changing to a higher adhesive grade and then pairing with continuous adhesive strips.
The story begins with a complaint phone call A printing factory in Central China that produces textbooks and teaching aids has been using the lowest priced bulk materials for a long time in order to reduce costsHot melt adhesive granulesI don’t usually see any problems, but every time we ship in large quantities during the […]
Guangzhou Sunlife wishes everyone a happy May Day holiday! 2022- Guangzhou Sunlife May Day holiday notice: According to the regulations of national statutory holidays and combined with the actual situation of the company, the holiday arrangement for May Day 2022 is hereby notified as follows:From April 30, 2022 to May 4, 2021, there will be […]
Recently, Secretary Guo of the Shishan Town Committee of Nanhai District and his team, accompanied by the community’s responsible person, conducted an on-site inspection of Foshan Jucai New Materials Co., LTD. This inspection aims to gain a thorough understanding of the production and operation status of enterprises and promote the upgrading and innovative development of […]
Background: The bottleneck of binding due to seasonal rush work A factory that produces cultural and creative calendars focuses on rushing goods in the fourth quarter of each year. Originally, the main line was dried with cold glue,Hot melt adhesive granulesAfter being put into operation, the speed should have been increased, but the yield rate […]