新闻中心
A express packaging factory in Hangzhou produces 500000 corrugated cardboard boxes per month and has been relying on experience to use themhot melt adhesive pelletsSeal the box with approximately 3 grams of glue per box. After switching to Sunlife hot melt adhesive granules, the technical team helped them calculate the exact amount and found that 2 grams per box was enough – saving about 80000 yuan in adhesive costs per year.

Sealing and gluing usually use two glue lines (box cover+box bottom), with each glue line length=box width and a glue line diameter of about 1.5mm. Taking a standard express box 40cm × 30cm × 20cm as an example:
Originally, 3g/box was a serious overspray, and the glue line was too thick, which resulted in glue overflow and unsightly appearance. After adjusting the spacing between the glue heads and the glue dispensing speed, the adhesive strength of 2g/box fully meets the standard.
Q: How to determine if the amount of sealing glue is sufficient?
A: Flipping the cardboard box and vigorously shaking it until the glue line does not open is considered qualified. A more scientific approach is to conduct a drop test (1.2m free fall without opening the box).
Q: What is the difference in the amount of glue used between small and large boxes?
A: Directly proportional to the length of the glue line. The small box (20cm wide) weighs about 0.7g/piece, while the large box (60cm wide) weighs about 2.1g/piece. Calculating based on actual dimensions is more accurate than estimating.
According to the notice issued by The State Council on the New Year’s Day holiday in 2022 and in light of the actual situation of our company, the holiday arrangement for New Year’s Day of our company this year is as follows: From Saturday, December 31, 2022 to Monday, January 2, 2023, there will be […]
Customer confusion: Two types of adhesive particles are too troublesome A book and magazine printing factory in Zhejiang Province uses both back adhesive (high flowability EVA) and side adhesive (fast curing EVA) on the adhesive assembly linehot melt adhesive pelletsTwo glue pots, two sets of temperature controls, changing glue and cleaning are time-consuming and laborious. […]
Direct answer: The real reason for the intermittent sealing line on this sealing line is the bridging of the feeding port of the melt glue pot, which causes the liquid level to intermittently decrease, and the carbonization residue inside the nozzle is partially blocked. After cleaning the pot and changing the material+adjusting the feeding method, […]
A factory that exports precision instruments used BOPP tape to fix honeycomb cardboard liners. However, due to rough shipping, the liners shifted and instrument edges were damaged, resulting in a high return rate. Later, it was changed toHot melt adhesive particles are glued and fixedLet’s break down this set of tactics and talk about it. […]