新闻中心
At the end of 2025, a large textbook printing factory explicitly requested in the bidding documenthot melt adhesive pelletsThe supplier provides a shear strength test report. After receiving the request, Guangzhou Sunlife’s commercial and technical department went through the standard testing process from sample preparation to report issuance. The following are the actual test records.

Referring to GB/T 7124-2008 (Method for determination of tensile and shear strength of adhesives), the test piece is overlapped with 150mm × 25mm × 2mm plywood, with an overlap length of 12.5mm and a glue layer thickness of 0.1mm. The universal testing machine has a tensile speed of 10mm/min. Take the average of 5 parallel samples per group.
Test results: The shear strength of Sunlife hot melt adhesive particles SL-268 standard type is 2.8MPa, and the shear strength of SL-368 high viscosity type is 3.5MPa, both far exceeding the industry standard requirement of ≥ 1.5MPa for book binding. The strength retention rate after high-temperature aging (80 ° C × 72h) is greater than 85%.
The technical director of the printing factory said, “Previously, we only looked at the viscosity parameters of the glue, but this measured data has given us a quantitative understanding of the long-term reliability of the glue, and we have more confidence in the selection
Q: What is the difference between shear strength and peel strength?
A: Shear strength is measured parallel to the adhesive surface (simulating spine tension), and peel strength is measured perpendicular to the adhesive surface (simulating flipping and tearing). Both book and magazine binding are important, but cutting is even more crucial.
Q: How can I test without a universal testing machine?
A: It can be sent to third-party testing institutions (such as SGS, CTI) at a cost of approximately 500-1000 yuan per group. Sunlife hot melt adhesive granules have internal testing data for each batch of production, which can be requested from the technical department.
Oil resistance testing caused by food packaging returns A certain food packaging factory received a batch of returns: 2000 sealed paper boxes experienced seal delamination and leakage within 48 hours after being filled with edible oil. The factory director immediately suspected thathot melt adhesive pelletsQuality issue, but the problem persists even after changing to another […]
The problem starts with the logistics return order A home appliance factory in Foshan that produces heaters and small refrigerators experienced concentrated complaints during the peak winter season last year: nearly 2% of the cardboard box covers of goods shipped to the north were lifted or even completely cracked after arriving at the warehouse. The […]
The cause of the matter A color box factory in Dongguan prepared 3 tons of paste boxes before the peak seasonHot melt adhesive granulesOn the second day of arrival, the operator reported that the glue color was noticeably yellowish compared to the previous batch, and faint glue marks could be seen on the edges of […]