新闻中心
EVA hot melt adhesive is currently one of the widely used industrial adhesives. They are essentially thermoplastic based on polymers, which means they are solid at room temperature but liquefy when exposed to a heat source.
In this article, you will learn more about hot melt adhesive: EVA hot melt adhesive. What issues should be noted when using?
Do you use different types of hot melt adhesives to bind different types of paper?
Sure, ordinary paper can be bound with ordinary hot melt adhesive and copperplate paper adhesive. Copperplate paper adhesive needs to be bound with copperplate paper; The glue pot of the wireless glue installation machine should use glue that has been open for a long time.
(Note: The opening time of hot melt adhesive refers to the time when the glue solidifies, which is generally 6-13 seconds.). )
2. How long should finished books be stored before cutting?
Cutting should be carried out during the cooling, hardening, and forming process of hot melt adhesive. Generally, this time should be kept at least 3 minutes, otherwise problems such as spine deformation and adhesive sticking may occur.
(Note: The cooling and hardening time of EVA hot melt adhesive is generally more than 3 minutes)
3、 How should the temperature of the glue tank be adjusted?
Firstly, the technical specifications provided by the Sunlife hot melt adhesive manufacturer must be followed. Too high or too low will reduce the adhesive strength and tensile strength. Therefore, the temperature of the hot melt adhesive particles must be controlled within a certain range to achieve adhesion.
In addition, the temperature of the adhesive should vary depending on the quality of the paper. For example, the inorganic content in copperplate paper is about 10 times higher than that in adhesive paper and writing paper. Inorganic substances have good thermal conductivity and can accelerate the cooling of hot melt adhesive particles;. The curing speed, so in this case, the temperature of the glue pot should be slightly increased.
What are the requirements for the use environment of EVA hot melt adhesive?
In general, maintaining a temperature of 20-25 ℃ and a humidity of around 50% can achieve the bonding effect.
5、 How long does it take for books and magazines to be delivered for use?
Usually shipped immediately at a digital printing store. Of course, there is no problem with regular use, but don’t read too much at this time because the bonding effect of EVA hot melt adhesive is only achieved after 24 hours.
6、 What are the common reasons for users to drop pages during use?
In addition to the issues mentioned above, it is usually necessary to pay attention to whether the equipment debugging is appropriate and whether the operation method is correct. Another easily overlooked issue is the addition of many adhesive particles at once during the operation process. However, due to the small workload each time, repeated heating and melting of EVA hot melt adhesive can damage the structure of the macromolecular chain and reduce heat generation. The viscosity of the melt. This situation is quite common in digital printing shops.
7、 Can edge glue and back glue be mixed?
Not recommended for mixed use. The fluidity of edge glue is higher than that of backing glue. Using edge glue as backing glue will make the book’s backing glue uneven and prone to empty glue. Back glue cannot be used as edge glue either.
8、 Why does transparent adhesive turn yellow?
Excessive temperature and prolonged repeated heating can cause the glue to turn yellow.
Solution: Reduce the temperature of the adhesive tank. When using hot melt adhesive particles at once, do not add too much. Use according to the amount and dosage, and if it is not enough, add more.
hot melt adhesive pelletsWhat should I do if I get damp? During the rainy season in the south or improper storage in the warehouse, the hot melt adhesive particles may absorb moisture. When damp rubber particles are heated, they will produce a large number of bubbles, overflow, and decrease in adhesion. But not all damp […]
The occurrence of wire drawing, back cracking, page dropping, or edge glue overflow in book and magazine binding lines may not necessarily be due to “insufficient glue”. The paper coating, glue temperature, glue amount, milling back quality, and finished product cooling time will all jointly affect the results. This article provides a feasible troubleshooting sequence […]
The flowability of hot melt adhesive particles has an impact on the quality of glue and adhesive. Hot melt adhesive has poor fluidity and can also cause stretching problems or mismatch with mechanical efficiency. 1. Sol temperature; Hot melt adhesive is very sensitive to temperature, and changes in temperature can alter the structure of the […]
Due to the fact that paper materials vary across different industries, we use different hot melt adhesives to bond the handles of paper bags, providing our customers with hot melt adhesive solutions for paper bags. This is not only for reinforcement but also to ensure the aesthetic appearance of the hand-held paper bags. More importantly, […]