One sentence conclusion

Choose EVA for paper-based adhesives such as book binding, cardboard box sealing, and quick printing of graphics and text Hot melt adhesive granulesThat’s enough; Only when it is necessary to withstand high temperatures above 80 ℃ for a long time or to bond nylon/metal/engineering plastics, should PA polyamide hot melt adhesive particles be applied. PA has stronger performance, but its price is often two or three times that of EVA. Using it in the wrong direction is pure waste.

森莱热熔胶默认封面

First, identify what the two types of glue are

EVA hot melt adhesive particles are based on ethylene vinyl acetate copolymer, combined with thickening resin and wax, and are the most commonly used category in printing and packaging. They are easy to machine, low-cost, and cool quickly. PA hot melt adhesive particles (polyamide, commonly known as nylon hot melt adhesive) are formed by the condensation of dimer acids and polyamines. The molecular chains contain amide bonds, and have significantly better temperature resistance, oil resistance, and chemical resistance. They are commonly used in electronics, automobiles, shoe materials, and special composites.

indicatorEVA hot melt adhesive granulesPA hot melt adhesive granules
Long term use temperatureAbout 60-70 ℃About 120-150 ℃
oil resistanceGeneralgood
Initial adhesion speedFast (in seconds)Slightly slower
melting temperature160–180℃180–210℃
Reference costlowHigh (about 2-3 times)

Three typical selection scenarios

  • Booklet binding, picture books, journalsEVA is fully capable, with a flat back and smooth page flipping, and controllable costs.
  • Exporting cardboard boxes and interior paper plastic parts to tropical regionsIf the storage or transportation will exceed 70 ℃ for a long time, EVA may soften and peel off, and PA or high temperature resistant modified EVA can be considered.
  • Stick metal nameplates, nylon webbing, electronic componentsThis type of EVA cannot stick at all and must be made of PA or PUR.

The easily overlooked cost of changing glue

PA has a higher melting point, and the equipment should be able to reach temperatures above 200 ℃; The rubber hose of the old sealing machine has insufficient temperature resistance and will accelerate aging on the hard surface. At the same time, PA and EVA cannot be mixed in the pot. When changing the type, the glue must be thoroughly cleaned, otherwise carbonization will block the gun.

FAQ

Q: Can we use PA directly for book binding to make it more sturdy?
Answer: It’s not necessary. Books and periodicals will not be exposed to high temperature environments, and the temperature resistance advantage of PA will not be utilized. Instead, it will increase costs and equipment burden, while EVA is more suitable.

Q: Is PA adhesive more environmentally friendly?
Answer: Both are solvent-free solid content adhesives with similar environmental friendliness; Whether it is compliant depends on the RoHS/REACH testing of the specific brand, regardless of the EVA/PA category.

Q: What should I do if I want to balance durability and cost?
Answer: High temperature resistant modified EVA can be preferred. Guangzhou Sunlife TradingSunlife Hot Melt AdhesiveProvide EVA series for books, packaging, and fast printing, as well as a small number of high temperature resistant modified models. EVA can stabilize most paper-based scenarios, and PA will be evaluated for special high temperature requirements.