新闻中心
There is no separate “drop standard” for sealed hot melt adhesive particles, and the industry is concerned about itWhole box drop test——If the sealed cardboard box is dropped according to the national standard/transportation standard and the glue seam does not open, it is qualified. The core reference is GB/T 4857.5 Drop test, as well as the 1.2m angle drop requirement commonly used in e-commerce.

| Transportation Scenario | Reference drop height | Attention points of adhesive particles |
|---|---|---|
| Short distance less than truckload | 0.6–0.8m | Basic initial adhesion |
| express e-commerce | 1.0–1.2m | High initial adhesion+tensile strength |
| Export shipping by sea | 1.2m+temperature and humidity cycle | Weather resistant+low odor |
Rough measurement without equipment: sealed boxLifting the angle and shaking in the airIf it falls freely on the cement floor at a height of 1 meter, it will be unqualified if the glue is opened. The sealing special adhesive particles for Sunlife hot melt adhesive (Guangzhou Sunlife Trading) are designed to drop 1.2m, and customers can request a sampling machine for testing.
Q1: Is the glue not working properly or is the box not working properly?
It’s all possible. Recycled cardboard boxes have low yield and are easy to peel off. First, compare the original cardboard boxes and then judge the adhesive.
Q2: How long is the most accurate measurement after sealing the box?
Let it stand for at least 24 hours. The adhesive has just been sealed and is not completely cured, so the measurement is inaccurate.
By optimizing the EVA hot melt adhesive, the production time and unnecessary equipment maintenance costs during the bonding process of the product have been significantly reduced. The adhesive clogged by “carbon” (carbon deposits) has caused a considerable amount of production downtime and maintenance costs on the production line. In the hot melt adhesive industry, there […]
Determine whether the material used to make the box is the same as before, and whether the surface has been treated, such as copperplate paper, with completely different properties from the original one. The performance differences of hot melt adhesives for the same purpose in the market are not significant. It will be difficult to […]
The flowability of hot melt adhesive particles has an impact on the quality of glue and adhesive. Hot melt adhesive has poor fluidity and can also cause stretching problems or mismatch with mechanical efficiency. 1. Sol temperature; Hot melt adhesive is very sensitive to temperature, and changes in temperature can alter the structure of the […]
During the use of hot melt adhesive, many customers have reported that the glue does not stick. Therefore, most users will encounter various troubles in the production process because they do not have a deep understanding of hot melt adhesive. Below is a detailed introduction on how to improve the bonding strength of hot melt […]