新闻中心
Direct answer: EVA hot melt adhesive granules are used for book and magazine packaging, and the glue pot is generally set at 160-180 ℃; The packaging and sealing scenarios are mostly between 150-170 ℃; The recommended construction temperature provided by the rubber particle manufacturer shall prevail, and the fluctuation should not exceed 10 ℃. The higher the temperature, the better. Long term overheating will cause the colloid to carbonize and turn black, and the adhesive strength will decrease.

The temperature of the glue pot directly determines the fluidity and opening time of the glue solution. Low temperature, viscous glue, uneven glue application, and easy occurrence of wire drawing and voids on the back of the book; If the temperature is too high, the oxidation of the glue will accelerate, and the bottom of the pot will coke and produce black slag, which will also shorten the service life of the hot melt glue particles. Guangzhou Sunlife Trading found during technical follow-up visits to graphic stores that over 60% of adhesive complaints were ultimately found to have improper temperature settings.
The first step is to set the median temperature according to the recommended temperature indicated on the packaging of the rubber particles; The second step is to test 10 bottles or 10 boxes of adhesive and observe the speed of wire drawing, penetration, and curing; Step three, adjust only 5 ℃ each time and run steadily for half an hour before making a judgment. Sunlife hot melt adhesive comes with recommended construction temperature parameters for each batch of products, which can be followed to avoid detours.
Q: Should the glue pot maintain its working temperature all the time?
It is recommended to lower the temperature to around 120 ℃ for insulation after stopping for more than 1 hour, which can save electricity and slow down the aging of colloids. After restarting and heating up for a few minutes, production can be resumed.
Q: Do I need to readjust the temperature when changing to different brands of rubber granules?
need. The softening point and viscosity temperature curve of different formulas are different. After changing the glue, the pot should be cleaned and the glue should be retested according to the recommended temperature of the new glue particles.
Summary: By setting the temperature according to the specifications of the glue particles, making small adjustments, and observing the glue line status frequently, the glue pot can be adjusted to the most suitable working point.
The packaging hot melt adhesive is heated to become liquid. Apply the liquid to the initial surface by extruding, spraying, or rolling the specified amount, and then expose it to a brief “open time” to achieve optimal temperature and “humidity” for bonding to the initial surface. After the designated opening time, the two surfaces come […]
How can EVA hot melt adhesive improve the safety of boxes and cartons? In addition to increasing production line speed to meet greater packaging demands, many box and carton factories hope to improve worker safety. Although this may require ensuring the use of appropriate hot melt adhesive at all times, the correct adhesive can have […]
Products that have been designed, perfected, manufactured, and inspected to ensure compliance with the highest standards. It’s time for packaging now. The last thing we want is a fragile container that will burst under harsh conditions such as storage, transportation, or shelving. After all, packaging is usually the first impression of a product on potential […]
Hot melt adhesive is not unfamiliar to cardboard packaging, as it is not only efficient but also cost-effective. Some packaging adhesives, equipment options, and packaging techniques were used when applying hot melt adhesive;. This article helps you understand the technology of hot melt adhesive suitable for your cardboard packaging. Conventional slotted cardboard box (RSC) Use […]