新闻中心
Hot melt adhesive granules are a type of plastic adhesive. Within a certain temperature range, its physical state changes with temperature, while its chemical properties remain unchanged. It is non-toxic and odorless. It is an environmentally friendly chemical product. Easy to package, transport, and store, solvent-free, pollution-free, and non-toxic. Some hot melt adhesives may encounter problems after long-term use. So how to deal with the problems encountered in hot melt adhesive packaging?
,Hot melt adhesive is non stick:
1、 Is hot melt adhesive tested before production. After long-term storage, the performance of hot melt adhesive is poor, the state is unstable, and it is prone to quality changes, which affects the performance of hot melt adhesive.
2、 The characteristics of hot melt adhesive. Due to insufficient permeability, it can affect the adhesion between books. The state and performance of hot melt adhesive are initially relatively stable, but over time, the page may fail and the adhesive interface may crack.
3、 Whether the production operation is correct. For example, the problem of paper falling off may not necessarily be a performance issue of hot melt adhesive. Before binding, it is necessary to check whether the hot melt adhesive can penetrate the surface of the book or magazine well. If the penetration is not good, it will affect the binding of books and publications. When folding and pressing after gluing, sufficient pressure and pressing time are required, otherwise it will also affect the performance of the hot melt adhesive.
2.Hot melt adhesive particles cannot produce glue:
1、 Has the hot melt adhesive particle been heated for a certain period of time before use? If used once a day, the hot melt adhesive should be preheated in the glue pot for 2 hours.
2、 Although hot melt adhesive particles are easy to use and maintain, they are also very durable. Usually, the shelf life of hot melt adhesive particles is 2 years, so it should be checked whether the hot melt adhesive has exceeded its service life.
Direct answer: Generally, high-strength spine glue is not used for bonding the inner pages of coil books. Instead, low-temperature or medium temperature EVA with shorter opening time (2-4 seconds), high initial adhesion, and good flexibility should be selected Hot melt adhesive pelletsThe softening point is between 80-90 ℃. Because the adhesive of the coil book […]
Hot melt adhesive technology features Fast solidification speed, solidifying within a few seconds, with the characteristics of heating, melting, cooling, and pasting, convenient for continuous and automatic high-speed operation, improving production efficiency and reducing costs; Hot melt adhesive particles have a 100% solid content, are solvent-free, environmentally friendly, non-toxic, energy-saving, and have no secondary pollution […]
The occurrence of wire drawing, back cracking, page dropping, or edge glue overflow in book and magazine binding lines may not necessarily be due to “insufficient glue”. The paper coating, glue temperature, glue amount, milling back quality, and finished product cooling time will all jointly affect the results. This article provides a feasible troubleshooting sequence […]
Lock wire glue=use glue casually? wrong! Many printing factories believe that books have already been sewn in,hot melt adhesive pelletsJust an auxiliary, just use cheap glue casually. This idea is completely wrong. The requirements for glue in the double process of wire locking and glue installation are actually more special. Please avoid the following three […]