Manual work (glue pot, hand-held glue gun repairing spine) and machine glue assembly line, forHot melt adhesive granulesThe requirements are in the opposite direction: manual work requires long open time and easy operation, while machine use requires fast initial adhesion and the ability to keep up with online speed. There is not a big problem with short-term emergency mutual use, but long-term mixed use will compromise both yield and efficiency.

| Dimension | Handmade use | Machine use (adhesive/sealing line) |
|---|---|---|
| Opening hours | Long, over 15 seconds, convenient for alignment | Short, 3-8 seconds, combined with high tempo |
| Melt viscosity | High, not easy to flow | According to the equipment specifications, it needs to be stable and pumpable |
| Initial adhesion force | Moderate is sufficient | High, press to shape |
| Resistant to repeated heating | High requirements (long-term insulation of the glue pot) | Fast cycle, relatively low requirements |
| Particle morphology | insensitive | Uniformity is required to prevent material blockage during loading |
It is recommended to prepare materials separately by workstation: the machine should be of the quick fix type, while the repair and sample book tables should be of the long open time type. Both should be labeled and stored separately to avoid mixing. Stores with small usage can only prepare one universal type, but they need to accept a compromise of compromise. Sunlife’s hot melt adhesive book series is available in both organic fast curing and manual long opening directions. Guangzhou Sunlife Trading can provide small batch combination supply solutions according to your workstation configuration.
If there is indeed a temporary shortage of materials that must be exchanged, the impact can be minimized by adjusting parameters: when using machine made quick fix materials for manual use, the glue temperature should be appropriately reduced by 5-10 ℃ and the amount of glue taken at a time should be reduced to save some operating time; If the manual long open material is temporarily placed on the machine, the pressing pressure should be increased, the holding time should be extended, and the line speed should be reduced. These are all emergency measures, and the corresponding brand should still be replaced after the order is fulfilled.
Q1: The graphic and text store only wants to prepare one type, which one should I choose?
If the machine is the main one, choose the machine with fast curing type. When repairing manually, reduce the glue temperature appropriately to extend the operable time.
Q2: Can two types of glue be mixed in the same glue pot?
Not recommended, compatibility and curing speed are inconsistent, which can easily cause delamination and affect strength.
As of April 29, 2024, domestic listed companies have successively released their annual performance reports for 2023. Adhesive Information has specifically compiled and summarized the operating performance data of listed companies in the adhesive industry for 2023. And based on revenue scale as the core indicator, the following “Top 10 Adhesive Listed Companies in China […]
Conclusion first: Exported books and periodicals need to be transported across the ocean, through high-temperature containers and temperature differences between high and low temperatures. Ordinary rubber particles are prone to sticking or becoming brittle during transportation, while weather resistant hot melt rubber particles have a higher softening point and a more balanced resistance to high […]
Matching principle in one sentence:The faster the machine speed, the faster the required curing and the shorter the opening time; If the machine speed is slow or the workpiece is large and needs to be aligned over a long distance, it should be fixed and opened slowly insteadChoosing the wrong direction is either due to […]
The reason why the adhesive layer is prone to cracking is related to the force and physical properties of the hot melt adhesive. Ultimately, it is still necessary to rely on hot melt adhesive to find the corresponding solution. Why does the magnitude of the force affect the fracture of the adhesive layer? Under normal […]