Many graphic and text store owners are afraid of changinghot melt adhesive pellets——Afraid of blocking rubber hoses, afraid of temperature switching problems, and afraid of wasting glue. In fact, as long as you follow the steps, it can be done in 15 minutes without stopping the machine for too long. The following is the standard glue changing process using Sunlife hot melt adhesive granules as an example.

Q: Can different brands of granules be mixed?
A: Not recommended. Mixing hot melt adhesive particles with different formulas may result in compatibility issues such as delamination and decreased adhesion. If a transition is necessary, rinse the hose thoroughly using steps 3-4.
Q: Does the first bound book always not stick firmly after changing the glue?
A: This is a normal phenomenon during the transition period of mixing old and new rubber residues in the hose. Squeezing 50-100g of mixed adhesive waste before starting formal binding can solve the problem.
Q: How often is it appropriate to change the glue?
A: It is recommended to clean the glue pot once a week and replace it with new glue every 1-2 weeks. If the glue is not replaced for a long time, repeated heating of the glue solution will cause severe aging, yellowing, and brittleness.
hot melt adhesive pelletsWhat should I do if I get damp? During the rainy season in the south or improper storage in the warehouse, the hot melt adhesive particles may absorb moisture. When damp rubber particles are heated, they will produce a large number of bubbles, overflow, and decrease in adhesion. But not all damp […]
The aging of hot melt adhesive is mainly manifested in two aspects: appearance and performance. Visually, the color of hot melt adhesive may become dull, and even yellow or brown tones may appear. The texture may become hard and brittle, losing its original flexibility, and the surface may have cracks or fissures. In terms of […]
Direct answer: FormalHot melt adhesive pelletsThe free sample sending process of manufacturers is usually “proposing requirements → explaining working conditions parameters → confirming sample model and quantity → sending for free (usually SF Express collect or free shipping for the first time) → customer testing on the machine → feedback results before adjustment”. The entire […]
When maintaining high-performance operation of the hot melt adhesive machine, you can take many measures to reduce downtime and improve system performance. Please remember that downtime equals production loss. 1) Apply hot melt adhesive at the correct temperature. Using the correct settings can avoid many troubles. You may also want to try using a metallocene […]