Sometimes when opening the glue bucket or opening the bound book, you may find that the hot melt adhesive turns yellow, brown, and even the back of the book becomes brittle. This is not just ‘glue color is like this’, it’s probablyExcessive heating or improper storageResulting in. Below are common reasons and prevention methods for yellowing and discoloration.


Sunlife hot melt adhesive is controlled for melting temperature and ratio according to the process card for each batch, matched with real model and batch testing, and tries to prevent “yellowing” before leaving the factory. If yellowing is found on the machine, don’t blame the glue yet – use a thermometer to measure the actual glue temperature, and most likely find the root cause of overheating; Confirmed to be a batch issue, Sunlife will replace the corresponding model according to the actual working conditions, provide the process card, and help you make the book back transparent and secure.
Q: Can the glue still be used if it turns yellow?
A: Those with slight color difference and no significant change in performance can be considered for use up; If it has become brittle, brushed, and cannot stick firmly, it indicates severe carbonization. It is recommended to clean the pot and change the batch, and do not compromise.
Q: Is yellowing and moisture clumping the same thing?
A: No, it’s not. Yellowing is mostly caused by high-temperature carbonization/oxidation; Dampness causes clumping, bubbles, and white spots on the machine. Both rely on “temperature control+good storage” for prevention.
Q: How to quickly determine if it is caused by overheating?
A: Measure the true temperature of the glue pot with a thermometer. If it exceeds the 160-180 ℃ marked on the process card, it is basically due to overheating carbonization and yellowing; After calibrating the temperature, observe whether the color of subsequent batches has recovered.
The yellowing and discoloration of hot melt adhesive are most likely caused by “overheating carbonization”, prolonged boiling, batch oxidation, and improper storage. By calibrating the temperature, monitoring the batch, and ensuring stable warehouse management, the adhesive can remain transparent and firmly adhered.
Product features of EVA Hot melt Adhesive: Biodegradable: Discarding or incinerating it is harmless to the environment. The price is similar to that of PVC: EVA is more expensive than toxic PVC, but cheaper than PVC without phthalates. Lighter in weight: The density of EVA is 0.91-0.93, while that of PVC is 1.32. Odorless: EVA […]
Why is it important to control the liquid level of the melt glue pool? The liquid level of the adhesive pool on the book binding line and sealing line directly affects the stability of the adhesive: low liquid level → intermittent adhesive release, uneven adhesive layer; Excessive liquid level → overflow of glue, accelerated aging […]
Why is it easy to have problems with spine fabric bonding The adhesion of the spine cloth (gauze/mull) in hardcover books is the most technically advanced part of the binding process: the spine cloth should stick to the back of the book, adhere to the shell surface, and ensure that the spine cloth does not […]
Answer directly The surface of laminated business cards is dense and has low polarity, making it easy to “fake stick” when directly glued. The key is to choose the right adhesive type, treat the surface well, control the temperature and pressure, in order to stick firmly. Operating Steps Choose adhesive:Used for adhesive film and PVCHot […]