The first few books and cardboard boxes couldn’t stick firmly when turned on, but then it became normal – this is almostHot melt adhesive granulesThe most common phenomenon in use. The root cause is usually that the temperature displayed on the glue cylinder has reached, but the glue has not yet fully penetrated, or there are still old glue cold sections left in the pipeline or nozzle from the previous time. Misunderstanding glue as having problems and repeatedly changing materials often results in wasted money.

| Steps | key points |
|---|---|
| 1. Preheat in advance | Power on 20 minutes earlier than working hours |
| 2. Constant temperature standing | After reaching the temperature, wait for 10-15 minutes for the glue to heat up completely |
| 3 rows of old adhesive | Empty 3-5 times, remove the degraded old glue completely |
| 4. Test the first piece | Conduct a test pull, and if it meets the requirements, proceed with mass production |
| 5 small amounts of frequent addition | Feed in batches to maintain stable cylinder temperature |
Sunlife hot melt adhesive comes with a brand and process card, indicating the recommended adhesive temperature and preheating time; Guangzhou Sunlife Trading can also assist in organizing the startup process into workshop dashboards to reduce the pitfalls of shift handover.
If there is a downtime of more than one hour during lunch break or shift handover, it should also be treated with “constant temperature and glue discharge” when starting again, and cannot be directly continued. It is recommended to use up or drain the remaining glue in the rubber cylinder as much as possible before the long holiday shutdown, to avoid long-term high-temperature insulation that may cause the entire cylinder to degrade and coke. Starting up after the holiday is both time-consuming and prone to clogging. A signboard next to the equipment indicating the preheating time and the number of adhesive discharges is much more reliable than verbal handover.
Q1: Is it considered a defect if the first board is not firm after replacing with a new brand of adhesive?
First, follow the preheating and rubber removal process according to the temperature of the new brand, and most of them will recover; Still unable to contact the supplier for parameter review.
Q2: Can the scrapped parts on the first board be recycled?
Paper products are not recommended to be returned to the furnace as the glue has contaminated the paper fibers. It is safer to dispose of them directly.
What is hot melt adhesive? Hot melt adhesive is the name of any polymer based adhesive applied in a molten state. The application of adhesives is usually through industrial glue guns, which act by triggering actions or finger pressure. Due to its versatility, hot melt adhesive is used in various environments, including packaging, binding, carton […]
During the use of hot melt adhesive, many customers have reported that the glue does not stick. Therefore, most users will encounter various troubles in the production process because they do not have a deep understanding of hot melt adhesive. Below is a detailed introduction on how to improve the bonding strength of hot melt […]
Conclusion The amount of glue used is small, and there are many varieties (books, packaging, and quick printing require a little each). Buying each item alone cannot meet the minimum order quantity, and the unit price is high. Using “mixed batch and combined order” – combining multiple categories of orders from the same supplier, or […]
EVA hot melt adhesive is currently one of the widely used industrial adhesives. They are essentially thermoplastic based on polymers, which means they are solid at room temperature but liquefy when exposed to a heat source. In this article, you will learn more about hot melt adhesive: EVA hot melt adhesive. What issues should be […]