新闻中心
The raised edges after composite should not be directly attributed to glue. This article investigates the interfaces of substrate, coating, composite, and curing one by one, helping to narrow down the scope of problems in packaging production sites.
Core keywords: packaging composite adhesive, edge warping, composite process, substrate surface Sunlife

The edge of the composite film tends to curl up after winding or before entering the next process. If the amount of glue is immediately increased at this time, it may mask the real problem and bring risks to appearance, cost, or subsequent processing.
You can investigate in the following order.
Firstly, check if the substrate is consistent. Confirm whether there have been any changes in the front and back, surface condition, storage time, and incoming batch of the same roll of material. If the problem is only concentrated on a certain batch of substrates, priority should be given to retaining the samples and verifying with the supplier.
Secondly, check if the coating is uniform. Observe whether there is a significant difference in the adhesive state between the edges and the middle, and check whether the coating components, guide rollers, and tension are stable. Edge problems may not necessarily come from the adhesive itself, but may also be related to the contact state of the equipment.
Thirdly, observe the bonding conditions during the composite process. Check whether the composite pressure, feeding status, and winding tightness are consistent with normal production. Uneven force distribution at the edges of the material may result in different bonding effects compared to the middle.
Fourth, look at the time when the problem occurred. Appears immediately after recombination, after placement, and after slitting, corresponding to different investigation directions. Matching the appearance time with the on duty record is easier to determine than just looking at the finished product.
When handling on-site, it is recommended to first fix a variable for small-scale verification, and not adjust the glue amount, speed, and equipment conditions simultaneously. For new substrates, new structures, or abnormal batches, the control samples should be retained to avoid directly scaling up production based on experience.
Sunlife can assist in selecting materials based on actual substrate and process requirements, providing sample testing, stable supply, and technical support. When communicating with procurement and process personnel, the substrate name, composite structure, abnormal location, and stage of problem occurrence should be provided simultaneously to make testing more targeted.
FAQ:
ending:
Breaking down the problem into interfaces for item by item confirmation is often closer to an effective solution than simply “changing a bucket of glue”. Sunlife can cooperate to complete sample verification and subsequent technical communication for the selection of packaging composite adhesive and on-site abnormalities.
Direct answer: The impact is significant. For every 10 ℃ decrease in workshop temperature,hot melt adhesiveThe actual opening time has been reduced by about 30-40%; When the relative humidity exceeds 75%, the moisture content of the paper increases, and the wetting and penetration of the adhesive will deteriorate. The performance of the same batch of […]
How to solve the problem of EVA hot melt adhesive becoming brittle in winter and cracking in summer? Summer is coming soon, and many new factory owners may not have encountered this problem before. There are also some who have encountered similar problems, but they were solved by our factory arranging technical personnel to help […]
How to use hot melt adhesive in the assembly of filter cartridges? Effective filtering is becoming increasingly important in today’s world. Whether it’s the air at home, drinking water in the city, or fuel in heavy vehicles – filters are required to do more. Hot melt adhesive for filter cartridges is essential in filter assembly. […]
Hot melt adhesive granulesHow much does one ton cost? Hot melt adhesive particles are priced by ton, but the price range is wide: ordinary EVA book/seal particles are mainly priced at around 9000-14000 yuan/ton, while modified, low-temperature fast curing, or PO specific particles may be priced at 15000-22000 yuan/ton. The price is not determined by […]