新闻中心
Firstly, the result is that a high-end mooncake gift box factory often has curled edges and peeling glue on the pasted dough paper and box corners when making high-end mooncake gift boxes. After switching to Sunlife hot melt adhesive for fine decoration and pasting, adjusting the opening time and gluing process, the box corners fit snugly without warping, and the top and bottom covers fit smoothly. The return rate has decreased from 3% to below 0.5%.

The factory will send the box samples and tissues to Guangzhou Sunlife Trading. The technical judgment problem lies in the short opening time and insufficient initial adhesion, which caused the corners to solidify before the adhesive was compacted. Solution: Use special adhesive particles for fine decoration pasting with longer opening time and mild initial adhesion to facilitate workers to easily package corners and align them; Accurate control of the amount of glue applied to avoid glue overflow and penetration; Apply appropriate pressure at the corners to ensure a snug fit. The first batch of 200 sets will be tested, and after passing the fitting, flipping, and storage tests, the quantity will be measured.
| indicator | Before changing the adhesive | After changing the adhesive |
|---|---|---|
| Box corner curling/glue opening | About 3% | Less than 0.5% |
| Overflow glue and penetration glue | occasional | Basic elimination |
| Heaven and earth cover fitting | Unequal tightness/looseness | Smooth and consistent |
The key to choosing glue for the high-end box of the Heaven and Earth Cover is twofold: first, the opening time should be long enough to allow time for manual corner alignment; The second is the balance between initial and final adhesion, which can both locate and firmly adhere. The film coated paper also requires a high initial adhesion formula. Guangzhou Sunlife Trading can recommend corresponding models based on the paper material and process rhythm.
Q: Can the Tian Di Gai gift box be sealed with ordinary rubber granules?
Not recommended. The opening time of the sealing rubber particles is short, the initial adhesion is rapid, and it solidifies before the corners are aligned, making it easy to curl the edges. A special formula is required for fine decoration and pasting.
Q: What should I do if the coated paper always doesn’t stick firmly?
The film layer is smooth, and it is necessary to choose Sunlife hot melt adhesive special models with high initial adhesion and adhesive film coating, and apply pressure at the corners to significantly improve the bonding effect.
The experience of this case is that the edge curling and glue opening of the deluxe gift box often do not match the opening time and initial bonding process well. Choosing the right specialized adhesive particles can solve the problem.
Direct answer:hot melt adhesiveThe correct usage of particles can be concentrated into six steps – selecting the type according to the live parts, controlling the temperature within the recommended range, adding small amounts multiple times, controlling the opening time for pressing, keeping the glue pot clean, and not repeatedly returning the remaining glue to the […]
First of all, let’s talk about the results: a tourism printing factory in East China produces foldable map brochures, with 55 gram ultra-thin floor drawings on the inner pages. Originally, using ordinary rubber particles often resulted in glue penetration and cracking at the folds. After switching to Sunlife hot melt adhesive thin paper special low-temperature […]
The force, material combination, and equipment rhythm borne by the lifting rope, side edges, and bottom adhesive of paper tote bags are not completely the same. When choosing hot melt adhesive for hand-held bags, the spraying method, pressing cycle, paper material, and usage environment should be clearly explained first, and then the matching degree between […]
Speed up=page drop? In March 2026, a textbook printing factory in Wuhan increased the speed of the glue line from 400 books/hour to 600 books/hour in order to meet the autumn textbook orders. As a result, the page drop rate skyrocketed from 0.3% to 4.2%, with almost 1 out of every 25 books experiencing page […]