新闻中心
Many packaging factories only conduct peel tests at room temperature of 25 ° C and pass if they feel they cannot be peeled off. In fact, the transportation of color printed corrugated cardboard boxes requires extreme conditions such as high temperature carriages (50 ° C+), cold storage (-18 ° C), and high humidity environments. Being qualified at room temperature does not necessarily mean being reliable under all operating conditions.

The correct approachAdd at least two testing points, high temperature of 50 ° C and low temperature of -10 ° C, to simulate real transportation conditions.
During the drop test, many people only check whether the cardboard box is cracked, ignoring whether the sealing glue line is displaced or detached. The cardboard box is intact but the glue line has been displaced, making it easy to unpack during subsequent transportation.
The correct approachAfter falling, measure the displacement of the adhesive line with a caliper. If it exceeds 2mm, it is considered unqualified; Simultaneously conduct a secondary drop test to verify the fatigue resistance of the adhesive wire.
Increasing the amount of glue applied to corrugated cardboard boxes does not increase the bonding strength nonlinearly – the incremental returns decrease after exceeding 60g/m ², and excessive glue can penetrate the corrugated core paper, leading to a decrease in cardboard strength and ultimately reducing the overall compressive strength of the cardboard box.
The correct approachThe optimal range for glue application is between 40-55g/m ², and proper placement of glue points is more effective than simply adding glue. Sunlifehot melt adhesiveThe sealing special model can achieve the tearing strength of corrugated paper with a coating amount of 40g/m ². Guangzhou Sunlife Trading can provide standard test samples and testing method guidance.
For most terminal packaging operations, adhesive carbonization is usually the main cause of most downtime events. Once EVA hot melt adhesive carbonization occurs, it will be difficult to clean thoroughly without taking extreme measures. Even after flushing, charcoal may still stick to narrow corners and continue to cause issues that affect normal operating time and […]
The glue thread is too long and the tail is shaking glue, which is not because the glue is “bad”, but because the opening time, temperature, and glue amount are not properly matched. According to these three inspections, most of the wire drawing problems can be solved.
Products that have been designed, perfected, manufactured, and inspected to ensure compliance with the highest standards. It’s time for packaging now. The last thing we want is a fragile container that will burst under harsh conditions such as storage, transportation, or shelving. After all, packaging is usually the first impression of a product on potential […]
What are the properties, costs, and functions of hot melt adhesive? Many different materials are used to produce different hot melt adhesives. The final performance of hot melt adhesive indicates that there are significant differences in the cost, performance, and functionality of the final product of hot melt adhesive. Tape and label hot melt adhesive […]