新闻中心
Why does EVA hot melt adhesive have wire drawing? Occasionally, when the nozzle of the equipment is turned off, there may be a small amount of filament residue, causing equipment contamination or sticking to the side of the guide rod, pressure plate, etc., which can cause problems with the appearance and operation of the box that needs to be carried out.
After observing and analyzing this phenomenon, as well as the opinions of industry experts, the main reasons for EVA hot melt adhesive can be attributed to the following aspects:
It is crucial to choose the appropriatehot melt adhesivefor each application. The adhesive required to complete a specific task may vary greatly, so it is important to understand which adhesive is most suitable for your application. The five commonly used types of main polymer substrates are the main components of our paper boxes and box […]
Using hot melt adhesive particles on the same material surface will provide better quality assurance, as hot melt adhesive is always sprayed on the material surface in a molten state – this helps to generate thermal reactions and increases adhesion compared to adhesives, without using heat during the bonding process. Stable quality provides good adhesion […]
Conclusion: Complianthot melt adhesiveParticles are basically non-toxic at room temperature, and the risks mainly lie in “high-temperature melting” and “ingestion” Conventional EVA and APAO based hot melt adhesive particles are 100% solid content, solvent-free bulk adhesives that are stable at room temperature, non-volatile, and safe for daily contact and storage. What really needs to be […]
The feasibility of reheating and reworking hot melt adhesive after solidification depends on the degree of degradation of the adhesive performance after the secondary heating. This article explains the typical changes of EVA hot melt adhesive after multiple heating, the key points of rework operation, and why PUR cannot be reworked.