新闻中心
On bound bookshot melt adhesiveTo remove it, the correct approach isFirst, control the temperature to soften, then mechanically separate, and finally clean the residual glueUsing a mild heat source of 60-80 ℃ to soften the adhesive layer and peel it off as a whole is more secure than any forced tearing or chemical pesticides. Unfortunately, in practical operation, most people fall into these pitfalls as soon as they come up.

The cohesive strength of hot melt adhesive at room temperature is often higher than that of paper, and the result of hard tearing is that the paper is torn apart and the adhesive remains on top. Especially for old books, the paper has become brittle and the corners are missing when torn. The correct approach is to first heat and soften the adhesive to make it “stretchable” before slowly separating it.
The temperature of the air gun can easily exceed 300 ℃, causing the paper to become burnt, yellow, curled, and ink to bubble and transfer. Suggest using a low-grade hair dryer or iron to cushion the leather paper, controlling it at 60-80 ℃, and tentatively lifting it while heating.
Strong solvents have limited effect on EVA hot melt adhesives, but they can easily dissolve ink and film, causing the cover to be scrapped and posing a risk of irritating volatile compounds. If chemical assistance is necessary, a small area test should be conducted in an inconspicuous location on the back of the spine first.
Low temperature brittleness can indeed cause some adhesive layers to break easily, but it has a negative effect on the flexibility of book and magazine type adhesive particles, and the paper will wrinkle when it gets damp after freezing. The freezing method is only suitable for small areas of adhesive residue and is not suitable for the entire spine of a book.
The residual adhesive layer has poor compatibility with the new adhesive layer, which can form a sandwich layer and almost inevitably cause secondary cracking. After milling or scraping off, the spine of the book should be polished with fresh fibers and then coated with new glue.
The root cause of a large number of repairs is usually a mismatch in the first use of adhesive – insufficient opening time, high softening point selection, or excessive adhesive layer. Sunlife hot melt adhesive from Guangzhou Sunlife Trading is supplied in separate lines for books, packaging, and graphic printing, and provides recommended parameters for adhesive quantity and temperature to help customers use “repair rate” instead of “unit price” as the accounting standard.
Q: Can hot water soak books to remove glue?
Answer: Not recommended. Paper deformation is irreversible when it comes into contact with water, and the benefits outweigh the losses.
Q: Can the removed old glue be recycled?
Answer: There are many residual adhesive impurities mixed with paper fibers and ink, and it is not recommended to return them to the furnace for production.
plum rain seasonHot melt adhesive granulesAgglomeration, mostly not due to glue spoilage, but ratherMoisture absorption+temperature fluctuationCausing mutual adhesion between particle surfaces. The principle of handling is simple: mild adhesion can be spread out and left to air, and after being dispersed, it can be used as usual; If there is obvious moisture absorption, whitening or […]
The acceptance of pearl cotton hot melt adhesive should not only focus on whether it sticks when just pressed. For the processing of cushioning packaging, lining, and combination packaging, appearance, positioning, and adhesive performance after cooling are equally important as batch operation stability. This article provides a practical on-site judgment method. Core KeywordsPearl cotton adhesive, […]
The core of Guangzhou flatbed hot melt adhesive isMoisture and heat resistance, good leveling, strong initial adhesion, and adaptable opening timePriority selectionModified EVA (mass production) or PUR (high-end)Accurately match according to the substrate, equipment, and season, avoiding “soft in summer and brittle in winter, opening glue in the south”. 1、 Guangzhou climate pain points (key […]
How often is it appropriate to clean the glue pot? The cleaning cycle of the glue pot depends on the amount and type of glue used. General recommendation: Thoroughly clean every 2-3 months under continuous production conditions; Intermittent use (less than 3 days per week) can be extended to 4-6 months. But in the following […]