新闻中心
Compared to tape,Hot melt adhesive granulesThe seal is clean, residue free, and can pass through automatic lines, making it particularly suitable for food contact packaging such as lunch boxes, paper cup covers, and handbags. Selected correctly, both fast and stable.

| link | key points |
|---|---|
| Melt glue cylinder | Set at the recommended temperature for the brand, do not exceed the upper limit to prevent carbonization |
| coating weight | Sealing position 0.2-0.4 g/section, excessive glue overflow, insufficient opening |
| Press fit | After sealing, maintain pressure for 1-2 seconds before releasing |
| clear the machine | Clean the nozzle at the end of each shift and perform deep cleaning on weekends |
Sunlife hot melt adhesive packaging sealing granules provide food contact compliance versions. Guangzhou Sunlife Trading can send samples according to your box type for trial production before increasing the quantity.
Q1: Will there be oil or soup leakage after sealing?
Selecting the right model and controlling the coating amount, it is normal; The coating surface material needs to be confirmed to be adhesive.
Q2: How to break the seal when it becomes brittle in low temperature weather?
Replace with a low temperature resistant model or increase the adhesive temperature and pressure appropriately.
Is it more cost-effective to bind the instruction manual with saddle nails or glue? One sentence conclusion:Thin pages and small batch selection of saddle nails are more cost-effective; Having multiple pages, requiring high-end or long-term storage, the overall cost of adhesive packaging is better.The selection of manual binding should not only consider the processing fee […]
There is currently no single “universal national standard” for hot melt adhesive granules, but ratherProduct standards+method standards+safety and environmental protection standardsThe three types of documents together constitute the basis for acceptance. What the purchaser needs to master the most is which standard corresponds to each of the four indicators of softening point, melt viscosity, peel […]
Conclusion Coking in a melt glue pot is the result of prolonged exposure to high temperatures and oxidation and carbonization of the adhesive liquid in contact with air. Cleaning is divided into four steps: “cooling and emptying – physical scraping – solvent wiping – reset”. Usually, temperature control, covering, and regular glue replacement are used […]
The automatic sealing machine uses hot melt adhesive particles to seal the box, and the process can be summarized as six steps: cleaning and inspection → preheating with adhesive → setting temperature → adjusting the amount of adhesive sprayed → adjusting the sealing test → mass production. Novices can follow the instructions and get started […]