The first few books and cardboard boxes couldn’t stick firmly when turned on, but then it became normal – this is almostHot melt adhesive granulesThe most common phenomenon in use. The root cause is usually that the temperature displayed on the glue cylinder has reached, but the glue has not yet fully penetrated, or there are still old glue cold sections left in the pipeline or nozzle from the previous time. Misunderstanding glue as having problems and repeatedly changing materials often results in wasted money.

| Steps | key points |
|---|---|
| 1. Preheat in advance | Power on 20 minutes earlier than working hours |
| 2. Constant temperature standing | After reaching the temperature, wait for 10-15 minutes for the glue to heat up completely |
| 3 rows of old adhesive | Empty 3-5 times, remove the degraded old glue completely |
| 4. Test the first piece | Conduct a test pull, and if it meets the requirements, proceed with mass production |
| 5 small amounts of frequent addition | Feed in batches to maintain stable cylinder temperature |
Sunlife hot melt adhesive comes with a brand and process card, indicating the recommended adhesive temperature and preheating time; Guangzhou Sunlife Trading can also assist in organizing the startup process into workshop dashboards to reduce the pitfalls of shift handover.
If there is a downtime of more than one hour during lunch break or shift handover, it should also be treated with “constant temperature and glue discharge” when starting again, and cannot be directly continued. It is recommended to use up or drain the remaining glue in the rubber cylinder as much as possible before the long holiday shutdown, to avoid long-term high-temperature insulation that may cause the entire cylinder to degrade and coke. Starting up after the holiday is both time-consuming and prone to clogging. A signboard next to the equipment indicating the preheating time and the number of adhesive discharges is much more reliable than verbal handover.
Q1: Is it considered a defect if the first board is not firm after replacing with a new brand of adhesive?
First, follow the preheating and rubber removal process according to the temperature of the new brand, and most of them will recover; Still unable to contact the supplier for parameter review.
Q2: Can the scrapped parts on the first board be recycled?
Paper products are not recommended to be returned to the furnace as the glue has contaminated the paper fibers. It is safer to dispose of them directly.
By optimizing the EVA hot melt adhesive, the production time and unnecessary equipment maintenance costs during the bonding process of the product have been significantly reduced. The adhesive clogged by “carbon” (carbon deposits) has caused a considerable amount of production downtime and maintenance costs on the production line. In the hot melt adhesive industry, there […]
What is the reason why EVA hot melt adhesive does not stick? Some time ago, a customer asked us why we couldn’t stick books firmly when bonding. Through this small case, we will answer the question: What is the reason why hot melt adhesive does not stick? When bonding books, if EVA hot melt adhesive […]
Direct answer: One kilogram of hot melt adhesive granules specifically designed for books and periodicals, estimated to be able to hold approximately 80-120 books in a common A4 booklet (about 150 pages, with a book back length of about 29.7 centimeters); There are more pocket books and thin books, up to 150 or more; Thick […]
The weather resistance of hot melt adhesive affects its application effect. Hot melt adhesive manufacturers need to adjust the heat resistance of hot melt adhesive according to different application environments to achieve ideal application performance. The heat resistance of hot melt adhesive is closely related to its softening point. Hot melt adhesives with good heat […]