The surface of MDF is dense and smooth, with unclear fiber directionhot melt adhesive pelletsThe difficulty of bonding is higher than that of ordinary cardboard. The amount of glue applied is a key parameter – if there is less glue, it will not stick, and if there is more glue overflow, it will waste. Here are the reference coating amounts for three common scenarios.

Q: How to deal with edge overflow after bonding the density board?
A: Hot melt adhesive particle overflow can be scraped off with a silicone scraper during semi curing, and after complete curing, it can be removed by heating and softening with a hot air gun. Do not scrape hard in a cold state, as it may damage the surface of the board.
Q: Is the debonding of the edge of the density board due to insufficient glue or incorrect glue type?
A: Both are possible. First check if the adhesive amount meets the standard, and then confirm if the adhesive type is high initial adhesion type (PVC/ABS edge banding must use high initial adhesion type).
How much glue is needed to bond the density board? The surface of MDF is dense and smooth, with unclear fiber directionhot melt adhesive pelletsThe difficulty of bonding is higher than that of ordinary cardboard. The amount of glue applied is a key parameter – if there is less glue, it will not stick, and […]
Conclusion first: Factories with large daily shipments and automated production lines have lower comprehensive costs and better anti disassembly properties for sealing boxes with hot melt adhesive particles; For businesses that focus on small batches and manual packaging, adhesive tape is more flexible. The watershed is roughly 500 boxes per day – beyond this amount, […]
Direct answer: For paper bag rope adhesion, hot melt adhesive particles with high initial adhesion, good flexibility, and a softening point of 75-85 ℃ should be used. The diameter of the adhesive point should be 8-12mm, with one point at each rope hole. Press and hold for 3-5 seconds.The key is not in the amount […]
Hot melt adhesive particles “this batch is easy to use, the next batch will be overturned”, most likely due toBatch stability not controlledBelow is this5-Step Checklist for Arrival VerificationHelp you block fluctuations outside the production line. 1、 Verify ‘identity’ upon arrival 1. Batch number and reportVerify the factory batch number, COA (Composition Analysis Form), and […]