Why does pearl cotton hot melt adhesive have wire drawing? During the process of gluing pearl cotton with a drum hot melt glue machine, some customers may find that the hot melt glue has a wire drawing phenomenon. The wire drawing of the hot melt glue not only affects the construction efficiency, but also affects the appearance of the product, and may even affect the bonding effect. So how to solve the problem of hot melt adhesive wire drawing?
Possible reason 1: The temperature of the glue tank in the drum hot melt glue machine is too low
Reason and solution: Low temperature will increase the viscosity of hot melt adhesive, that is, the thinner it is, the easier it is to draw. The melting temperature of the hot melt adhesive machine can be appropriately increased to reduce the viscosity of the hot melt adhesive. It should be noted that the temperature of the hot melt adhesive machine should not be raised too high to avoid carbonization of the hot melt adhesive.
Possible reason 2: The glue is too thick
Reason and solution: The thicker the pearl cotton hot melt adhesive, the easier it is to draw. If the thickness of the adhesive is thin, the speed can be increased, and the higher the speed, the less adhesive is needed. You can also adjust the thickness knob to look thinner. Or adjust the pressing height during the gluing process, not too low or too low. The easier it is to draw.
Possible reason 3: The viscosity of pearl cotton hot melt adhesive is too high
Reason and solution: The higher the viscosity, the easier it is to draw. Replace low viscosity hot melt adhesive particles or replace special formula non brushed hot melt adhesive particles
Ordinary hot melt adhesive will draw, but the difference is obvious. When encountering wire drawing problems, there is no need to be nervous. Sunlife Hot Melt Adhesive has been dedicated to the research and production of hot melt adhesives for over a decade. We are dedicated to providing our customers with high-quality products and excellent value services.
What should I do if the hot melt adhesive particles are not firmly attached to the coated paper? Direct answer: The root cause of the poor adhesion of laminated paper is mostly due toLow membrane surface energy, glue not eating paper fibers, poor coordination between opening time and compressionThese three points. The surface of laminated […]
The occurrence of wire drawing, back cracking, page dropping, or edge glue overflow in book and magazine binding lines may not necessarily be due to “insufficient glue”. The paper coating, glue temperature, glue amount, milling back quality, and finished product cooling time will all jointly affect the results. This article provides a feasible troubleshooting sequence […]
The core of Guangzhou flatbed hot melt adhesive isMoisture and heat resistance, good leveling, strong initial adhesion, and adaptable opening timePriority selectionModified EVA (mass production) or PUR (high-end)Accurately match according to the substrate, equipment, and season, avoiding “soft in summer and brittle in winter, opening glue in the south”. 1、 Guangzhou climate pain points (key […]