In winter, when express cardboard boxes burst and open, it is mostly not due to poor quality of the glue, but rather the fact that the sealing glue that works well at room temperature becomes brittle and loses its stickiness in low-temperature environments. The solution is to replace it with a low-temperature resistant oneHot melt adhesive granulesAdjust the glue temperature and coating amount to the appropriate range, and pay attention to the moisture content of the cardboard box.

Ordinary sealed EVA adhesive will gradually harden and its impact resistance will decrease below 0 ℃, and it will crack upon impact. Special hot melt adhesive particles with the nominal “low temperature resistance/antifreeze” should be selected for sealing. This type of adhesive can be modified to press the brittleness temperature to -10 ℃ or even lower, and still maintain toughness at low temperatures. Sunlife Hot Melt AdhesivePackaging and Sealing SeriesThere are low-temperature models for e-commerce cold chain and winter in the north.
| link | Suggestion |
|---|---|
| Melt Temperature | 170-185 ℃, measured and calibrated, don’t just look at the panel |
| Rubber tube insulation | Maintain a constant temperature to avoid clogging the nozzle due to cooling |
| Environmental preheating | If the cardboard box is cold, warm it up first and then seal it for better glue penetration |
The moisture content of the cardboard box is too high, making it difficult for the adhesive to penetrate and prone to false bonding; If it is too dry, the glue will absorb quickly and the opening time will be shortened. The most stable range is 8% -12%. If there is dust or wax on the surface of the recycled cardboard box, it is necessary to first remove the dust or choose a glue with stronger adhesion.
Q: Can we raise the glue temperature to compensate for the low temperature?
Answer: No. Excessive temperature can only cause carbonization, wire drawing, and paper box ironing, but it can also be more explosive and damage equipment.
Q: Does the southern region also need low-temperature glue in winter?
Answer: If there is no heating in the warehouse, and the goods are transported to the north or cold chain, it is still recommended to use low-temperature models and choose according to the “worst transportation environment”.
Q: Do I need to change the equipment to change the low-temperature adhesive?
Answer: Usually not needed. The temperature range of most sealing spray glue machines is sufficient. Guangzhou Sunlife Trading can provide machine temperature and coating suggestions according to your model, and send samples to test one or two lines first.
One sentence: In winter, sealing the box without bursting the mouth=low temperature resistant rubber particles+calibrated rubber temperature+appropriate coating amount+controlling the moisture content of the cardboard box. Four steps together are necessary to ensure stability.
Hot melt adhesive granulesIs it normal to be soft in summer and hard in winter? This is a completely normal physical phenomenon. Hot melt adhesive particles are thermoplastic materials with a fixed softening point (usually between 70 ℃ -110 ℃). When the temperature in the warehouse is high and close to the softening point, the […]
Acrylic panels can be usedhot melt adhesive pelletsIs it sticky? Acrylic (PMMA) has extremely low surface energy and is widely recognized as a difficult to stick material. But by selecting the right type of hot melt adhesive particles and combining them with the correct surface treatment, it is entirely possible to achieve a firm bonding. […]
It is very important to understand the extensive application of adhesives in the packaging industry, including the formation and sealing of boxes, paper bags, cartons, labels, special applications, etc. All these applications share a common priority: ensuring the stability, safety and storability of packaged products, which helps to ensure that they do not yield to […]
EPE pearl cotton (foamed polyethylene) has a loose texture, poor high temperature resistance, and strong surface inertness, making it a difficult material to bond in the packaging industry. Ordinary hot melt adhesive is prone to problems such as melting through cotton, weak adhesion, low-temperature cracking, high-temperature delamination, pungent odor, and wire drawing affecting the appearance […]