Hot melt adhesive particles are hydrophobic but porous particles that will slowly absorb moisture after prolonged exposure after opening. The glue particles that have absorbed water are heated in the glue pot, and the water evaporates instantly into bubbles mixed in the glue, leaving pinholes and white spots after cooling; Water vapor also weakens the wetting of paper fibers by the adhesive, resulting in weak adhesion and falling pages.

| phenomenon | reason | consequence |
|---|---|---|
| Melt glue bubbles and overflows from the pot | Water vaporization and expansion | Uneven coating and waste |
| White spots and fogging on the adhesive layer | Residual water vapor forms micropores | Poor appearance and decreased strength |
| Adhesive adhesion decreases and pages fall off | Wetting is blocked by water vapor | Backbone/Box Opening Glue |
| Accelerated carbonization | Water catalyzed oxidation | Frequent gun blockage and machine cleaning |
Q: Does the nominal “moisture-proof” rubber particle not absorb water?
Answer: Moisture prevention is to delay or eliminate it. Long term exposure can still absorb moisture, and storage habits are the key.
Q: Will the performance of damp rubber particles recover after drying?
Answer: Mild moisture and drying can restore most of the performance; If it has clumped or turned yellow, the ingredients may have changed and it is not recommended to use it again.
Q: How can I ensure that the glue I bought is dry?
Answer: Choose products with sealed packaging and fast delivery. Guangzhou Sunlife TradingSunlife Hot Melt AdhesiveUsing moisture-proof inner lining bags, it is also recommended to store the goods in their original bags during the southern rainy season, use them as needed, and attach storage instructions to reduce the risk of moisture.
One sentence: High moisture content in rubber particles=bubbles, white spots, and weak adhesion. To prevent this, it is necessary to store it in a sealed environment and control the humidity. If it gets damp, it should be lightly dried and heavily scrapped.
Almost all factories that do book and magazine binding have encountered this frustrating problem: the production line is running, and the glue outlet of the glue binding machine suddenly breaks and is intermittent, or directly blocks the glue without dispensing, resulting in the opening, breaking, and uneven thickness of the glue layer on the books. […]
The raised edges after composite should not be directly attributed to glue. This article investigates the interfaces of substrate, coating, composite, and curing one by one, helping to narrow down the scope of problems in packaging production sites. Core keywords: packaging composite adhesive, edge warping, composite process, substrate surface Sunlife The edge of the composite […]
What are the characteristics of pearl cotton hot melt adhesive? Pearl cotton, also known as EPE, is a foamed polyethylene polymer. Pearl cotton has many advantages such as water and moisture resistance, shock resistance, sound insulation, thermal insulation, good plasticity, strong toughness, recycling, environmental protection, strong impact resistance, and good chemical resistance. Pearl cotton packaging […]
In the adhesive industry, rosin and modified materials are the most commonly used thickeners. Today, we will share some performance indicators of these resins: Rosin ① Name and characteristics Chinese alias: Tar rosin; Raw rosin. English name: Rosin. English alias: Symphony. Rosin is a transparent solid that is slightly yellow to yellow red in […]