新闻中心
Legitimate hot melt adhesive particles themselves are thermoplastic polymers that are solid, non-volatile, and insoluble in water at room temperature, making them relatively safe adhesive materials. Whether it is “toxic” mainly depends on the formula and high-temperature usage method.

| focus | Explanation |
|---|---|
| recyclability | Pure EVA hot melt adhesive belongs to thermoplastic and can theoretically undergo further hot melt treatment |
| Residual odor | After cooling, the odor is sealed, and there is almost no sensation when it comes to books/boxes |
| Inspection Report | Choose a manufacturer that can provide RoHS and VOC data |
Q: Can hot melt adhesive particles come into contact with food packaging?
Answer: It is necessary to choose a food grade formula and provide contact safety testing. Sunlife hot melt adhesive can provide corresponding reports according to its use.
Q: Does having a smell equate to being toxic?
Answer: Not necessarily, but a pungent smell usually means there are more volatile substances. It is recommended to replace it with qualified materials.
Q: How can the workshop reduce risks?
Answer: Temperature control should not exceed the upper limit, ventilation should be maintained, and low odor new material particles should be selected.
Sunlife hot melt adhesive from Guangzhou Sunlife Trading can provide environmental and food contact testing reports, making procurement more reassuring.
Direct answer: It can be used, but it is not recommended to exchange it for a long time Manual work (glue pot, hand-held glue gun repairing spine) and machine glue assembly line, forHot melt adhesive granulesThe requirements are in the opposite direction: manual work requires long open time and easy operation, while machine use requires […]
What does the length of the adhesive tape affect The problem of excessively long glue threads on the book and magazine binding line is a headache for the production line: the glue threads wrap around the book core, dirty the cover, and the glue breaks unevenly. In severe cases, each shift needs to be shut […]
Let me start with a true story that I’ve been remembering for eight years. In the winter of 2016, a printing factory owner called me at 11 a.m. and started off by saying, “Brother Shu, something big has happened. The 50,000 textbooks I just bound have their adhesive ridges broken on the first page. The […]
The true cause of blistering on the spine of a book The appearance of bubbles (visible bulges or internal cavities) on the spine of the adhesive book is a quality taboo, and customers will directly judge it as unqualified. Many people think that foaming is a problem with the glue coating process, but in realityhot […]