Coking in a melt glue pot is the result of prolonged exposure to high temperatures and oxidation and carbonization of the adhesive liquid in contact with air. Cleaning is divided into four steps: “cooling and emptying – physical scraping – solvent wiping – reset”. Usually, temperature control, covering, and regular glue replacement are used to prevent it. Don’t wait until the coke layer is thick before processing.

Switch the equipment to insulation or shutdown, wait for the adhesive solution to reach the operable temperature, and drain the adhesive tank of any still flowing adhesive. The coke layer is hard and brittle. Use a special scraper or copper shovel to gently scrape while it is warm, and do not scratch the pot wall with iron tools.
Remove the spray gun, filter screen, and hose, and soak them in matching cleaning agents or specialized decarbonization agents. Stubborn coke blocks can be softened and cleared by short-term heating, but avoid long-term air burning.
Dip a lint free cloth into a specialized cleaning agent to wipe off any residue in the pot until the surface of the cloth is basically clean. Note that the cleaning agent should be compatible with the material of the equipment to avoid corroding the seals.
Reinstall the components, add new glue and circulate at low speed, observe whether the glue is smooth and whether there are any black spots. It is recommended to remove the parts with residual coke at the front end during the first glue dispensing.
| Steps | key points | taboo |
|---|---|---|
| drain | Operation after temperature drop | Do not use iron tools to scrape hard |
| disassemble and clean | Decarbonization agent immersion | Avoid empty burning |
| wipe | Special cleaning agent | Do not corrode the seal |
| test run | Front end residual adhesive | Do not directly load the bulk order |
Q: How often do you clean the pot?
Answer: For continuous production, it is recommended to have a small cleaning every 1-2 weeks and a large cleaning every month. It is necessary to clean the formula before changing.
Q: Does the mixing of coke residue into the adhesive affect the bonding?
Answer: Yes, black spots block the gun, reduce its strength, and even dirty the back of the book. It must be cleaned.
Question: How to reduce coking?
Answer: Guangzhou Sunlife TradingSunlifehot melt adhesiveGood thermal stability, slow carbonization, combined with temperature control and covering, the cleaning cycle can be significantly extended.
Four steps to clear the pot, temperature control and covering regularly, coking is no longer a monthly nightmare.
Direct answer: The impact is significant. The direction of the book page threads should be parallel to the spine (straight), so that the paper is less likely to arch along the spine, the adhesive layer is evenly stressed, and the folding life is significantly longer; Books bound with horizontal threads have high page turning resistance […]
Hot melt adhesive is a type of plastic adhesive. Its physical state changes with temperature within a certain temperature range, while its chemical properties remain unchanged. It is non-toxic and odorless, and is an environmentally friendly chemical product. Hot melt adhesive is melted by heating. The molten adhesive turns into a liquid and is then […]
For a long time, assembly lines have been the most effective way to mass-produce almost all products. Of course, product assembly has been constantly improving. In recent decades, hot melt adhesives have become an indispensable part of the assembly process. Here are several ways in which hot melt adhesive is crucial to the success of […]
Hot melt adhesive has a certain degree of water resistance, but it is not waterproof adhesive. Short term dampness and high humidity are generally fine; Long term soaking in water will soften and loosen the adhesive. This article explains the water resistance boundary and unsuitable scenarios of EVA hot melt adhesive in one go.